Search

Common Titanium Welding Defects & Prevention

Welding defects: porosity, embrittlement, contamination.

Quick Answer

Porosity, embrittlement, discoloration, cracking. Inert shielding required above 250°C.

Weld Color Guide

Color Condition
Silver Excellent
Light straw Acceptable
Dark blue Reject
Grey/white Severe contamination

References

  • AWS D1.9, AMS 2680