Titanium Welding Guide: TIG, Laser, EBW Best Practices
Technical guide to welding titanium alloys: GTAW, laser, EBW.
Quick Answer
Titanium requires inert gas shielding above 250°C. GTAW is most common. Laser and EBW offer deeper penetration.
Process Comparison
| Process | Penetration | Speed | Cost |
|---|---|---|---|
| GTAW | 0.125 in | 6 ipm | Low |
| Laser | 0.250 in | 60 ipm | Medium |
| EBW | 2.000 in | 120 ipm | High |
References
- AWS D1.9, AMS 2680